Details

Title

Mechanical Properties and Fractographic Analysis of High Manganese Steels After Dynamic Deformation Tests

Journal title

Archives of Metallurgy and Materials

Yearbook

2014

Numer

No 3 September

Publication authors

Divisions of PAS

Nauki Techniczne

Publisher

Institute of Metallurgy and Materials Science of Polish Academy of Sciences ; Commitee on Metallurgy of Polish Academy of Sciences

Date

2014

Identifier

ISSN 1733-3490

DOI