Surface Analysis of Railway Buffers Heads Covered with Bronze Using Laser Cladding

Tytuł czasopisma

Archives of Foundry Engineering

Rocznik

2017

Wolumin

vol. 17

Numer

No 2

Autorzy

Słowa kluczowe

Wear resistant alloys ; Railway buffer heads ; Laser cladding ; Clads of aluminum bronze CuAl9Fe3 ; Properties of clads

Wydział PAN

Nauki Techniczne

Wydawca

The Katowice Branch of the Polish Academy of Sciences

Data

2017

Typ

Artykuły / Articles

Identyfikator

ISSN 2299-2944

Referencje

Lisiecki (2016), Tribological characteristic of titanium alloy surface layers produced by diode laser gas nitriding, Arch Metall Mater, 61, 543, doi.org/10.1515/amm-2016-0094 ; Lisiecki (2014), Welding of thermomechanically rolled fine - grain steel by different types of lasers, Arch Metall Mater, 59, 1625, doi.org/10.2478/amm-2014-0276 ; Gamon (2015), Movement analysis of cooperating railway buffer heads, Arch Trans, 33, 4, doi.org/10.5604/08669546.1160922 ; Jezierski (2014), Theoretical and practical aspects of pneumatic powder injection into liquid alloys with non - submerged lance, Arch Metall Mater, 59, 731, doi.org/10.2478/amm-2014-0121 ; Balogun (2014), Corrosion behaviour of alpha phase aluminum bronze alloy in selected environments ISSN, LEJPT, 24, 113. ; Janerka (2009), Quality of carburizers and its influence of carburization process Foundry, Arch Eng, 9, 249. ; Stojczew (2014), Melting of grey cast iron based on steel scrap using silicon carbide Foundry, Arch Eng, 14, 77. ; Węgrzyn (2016), Impact toughness of WMD after MAG welding with micro - jet cooling, Mater Technol, 50, 1001, doi.org/10.17222/mit.2015.159 ; Kurc (2016), Ozgowicz The microstructure of metastable austenite in steel after its strain - induced martensitic transformation, Mater Technol, 18, 10, doi.org/10.17222/mit.102

DOI

10.1515/afe-2017-0057

×