Abstract

<jats:title>Abstract</jats:title><jats:p>Microstructural characterization is an important tool to optimize the properties of engineering materials. Quantitative metallography is a common technique, which provides three-dimensional estimations of phases and structure elements from two-dimensional images. Metallography has been described as both a science and an art [</jats:p><jats:p>Superalloys are high-performance alloys which exhibits excellent mechanical strength and creep resistance at high temperatures, good surface stability, and corrosion and oxidation resistance. Temperature and corrosion resistant materials such as nickel-based superalloys are prepared mostly with standard metallographic techniques. However, the results can be significantly improved by using finely graded CMP (chemical mechanical polish) polishing solutions on a high napped polishing pad.</jats:p><jats:p>Sample preparation requires a certain degree of skills and experience, due to the high chemical resistance of most superalloys. Some chemical solutions are able to dissolve the</jats:p>

Publisher

Institute of Metallurgy and Materials Science of Polish Academy of Sciences ; Commitee on Metallurgy of Polish Academy of Sciences

Date

2017

Identifier

ISSN 1733-3490

DOI

10.1515/amm-2017-0086

×