Details

Title

Experimental Investigation and Multi-Response Optimization in Turning of Incoloy 800 H Superalloy

Journal title

Archives of Metallurgy and Materials

Yearbook

2018

Volume

vol. 63

Numer

No 4

Publication authors

Keywords

superalloy ; microstructure ; Taguchi- Grey approach ; mathematical models

Divisions of PAS

Nauki Techniczne

Coverage

1683-1691

Publisher

Institute of Metallurgy and Materials Science of Polish Academy of Sciences ; Commitee on Metallurgy of Polish Academy of Sciences

Date

2018.12.12

Type

Artykuły / Articles

Identifier

ISSN 1733-3490

DOI