Details

Title

Numerical modeling of fracture during nanoindentation of the TiN coatings obtained with the PLD process

Journal title

Bulletin of the Polish Academy of Sciences: Technical Sciences

Yearbook

2013

Volume

61

Numer

No 4

Publication authors

Divisions of PAS

Nauki Techniczne

Coverage

973-978

Publisher

Polish Academy of Sciences

Date

2013

Identifier

ISSN 0239-7528, eISSN 2300-1917

DOI