In order to determine the leading phase of the Fe - 4.25% C eutectic alloy, the method of directional crystallization, which allows to study the character of the solid / liquid growth front, was used. Examined eutectic was directionally solidified with a constant temperature gradient of G = 33,5 K/mm and growth rate of v = 125 μm/s (450 mm/h). The Bridgman technique was used for the solidification process. The sample was grown by pulling it downwards up to 30 mm in length. The alloy quenched by rapid pulling down into the Ga-In-Sn liquid metal. The sample was examined on the longitudinal section using a light microscope and scanning electron microscope. The shape of the solid/liquid interface and particularly the leading phase protrusion were revealed. The formation of the concave – convex interface has been identified in the quasi-regular eutectic growth arrested by quenching. The cementite phase was determined to be a leading phase. The total protrusion d is marked in the adequate figure.

Go to article

Authors and Affiliations

M. Trepczyńska-Łent
ORCID: ORCID
Download PDF Download RIS Download Bibtex

Abstract

The paper deals with the basic set-up of single-frequency microchip laser - so called Lyot filter configuration. Description of its operation and practical realization is given. Some results obtained for Nd:YAG/KTP microchip laser are presented. The evidences of single-frequency operation and its limits are emphasized. Described construction constitutes the base for building the frequency stabilization of green 532 nm microchip laser.

Go to article

Authors and Affiliations

A.J. Antończak
J.Z. Sotor
K.M. Abramski

This page uses 'cookies'. Learn more