Abstract

This paper is focused on the manufacturing and properties of light weight aggregates made from local waste materials. The waste materials were car windshield glass contaminated by PVB foil, fly ash, mine slates as well as wastes after toothpaste production. The main aim of the research was to combine car windshield glass and the aluminosilicate coal mine slates as a basis for light weight aggregates manufacturing. Fly ash were added in order to modify rheological properties of the plastic mass. Toothpaste wastes were introduced as a source of carbonates and CO2 evolution during thermal treatment. After milling and mixing all materials they were pressed and sintered at temperature range of 950°C-1100°C in air. The results show that it is possible to receive light weight aggregates only from the Silesian local waste materials. The significant influence of sintering temperature on properties of aggregates was observed.

Go to article

Authors and Affiliations

J. Smoleń
T. Pawlik
M. Sopicka-Lizer
D. Michalik
Download PDF Download RIS Download Bibtex

Abstract

This study focused on the reclamation of ash from incineration process and development of new artificial lightweight aggregate (LWA) that have comparable properties with existing natural coarse aggregate. The main objective of this study is to examine potential use of recycled municipal solid waste incineration (MSWI) ash as raw material in LWA production with a method of cold-bonded pelletization. Two types of incineration ash which is bottom ash (BA) and fly ash (FA) were collected from Cameron Highland Incineration Plant, Malaysia. The properties of BA and FA are studied by means of X-Ray Fluorescence (XRF) and microstructure of these ashes were inspected using Scanning Electron Microscope (SEM). The properties of BALA and FALA produced in this study is examined including loose bulk density, water absorption and aggregate impact value (AIV). From the results of both types of artificial LWA, the lowest loose bulk density of BALA is BALA50 with 564.14 kg/m3 and highest is at 831.19 kg/m3. For FALA50, lowest loose bulk density is 573.64 kg/m3 and highest is 703.35 kg/m3. Water absorption of BALA and FALA is quite similar with one another in with the value of 23.8% and 22.6%, respectively. Generally, FALA have better qualities of LWA comparing with BALA with lower bulk density and water absorption and can be categorized as strong aggregate. In summary, reclamation and reutilization of incinerator ash has generated acceptable qualities for artificial LWA. Both types of BA and FA shown a great potential to be recycled as additional materials in artificial aggregate production.
Go to article

Authors and Affiliations

Norlia Mohamad Ibrahim
1 2
ORCID: ORCID
Roshazita Che Amat
1 2
ORCID: ORCID
Mustaqqim Abdul Rahim
1
ORCID: ORCID
Nur Liza Rahim
1 2
ORCID: ORCID
Abdul Rahim Abdul Razak
3
ORCID: ORCID

  1. Universiti Malaysia Perlis (UniMAP), Faculty of Civil Engineering Technology, Perlis, Malaysia
  2. Universiti Malaysia Perlis (UniMAP), Faculty of Chemical Engineering Technology, Center of Excellence Geopolymer and Green Technology, Perlis, Malaysia
  3. Universiti Malaysia Perlis (UniMAP), Faculty of Electrical Engineering Technology, Perlis, Malaysia

This page uses 'cookies'. Learn more