Investigations of Microstructure of Resistance Spot-Welded Joints Made of HSLA340 and DP600 Steels / Badanie Mikrostruktury Złączy Zgrzewanych Punktowo Ze Stali HSLA340 I DP600

Journal title

Archives of Metallurgy and Materials

Yearbook

2012

Numer

No 4 December

Authors

Divisions of PAS

Nauki Techniczne

Publisher

Institute of Metallurgy and Materials Science of Polish Academy of Sciences ; Commitee on Metallurgy of Polish Academy of Sciences