Details Details PDF BIBTEX RIS Title Effect of Different Heat Treatments on Microstructure and Mechanical Properties of the Martensitic Gx12CrMoVNbN9-1 Cast Steel / Wpływ Parametrów Obróbki Cieplnej Na Mikrostrukture I Własciwosci Mechaniczne Martenzytycznego Staliwa Gx12CrMoVNbn9-1 Journal title Archives of Metallurgy and Materials Yearbook 2013 Numer No 1 March Authors Golański, G. ; Słania, J. Divisions of PAS Nauki Techniczne Publisher Institute of Metallurgy and Materials Science of Polish Academy of Sciences ; Commitee on Metallurgy of Polish Academy of Sciences Date 2013 Identifier DOI: 10.2478/v10172-012-0145-x ; ISSN 1733-3490