Details

Title

The Influence of Impurities in Feed Ingots on the Quality of Castings Made from Nickel Superalloy IN-713C

Journal title

Archives of Foundry Engineering

Yearbook

2013

Numer

No 4

Authors

Keywords

ATD ; Superalloys ; Feed ingot ; Master heat ; Solidification ; non-metallic inclusions

Divisions of PAS

Nauki Techniczne

Publisher

The Katowice Branch of the Polish Academy of Sciences

Date

2013

Type

Artykuły / Articles

Identifier

DOI: 10.2478/afe-2013-0073 ; ISSN 2299-2944
×