Details Details PDF BIBTEX RIS Title Evaluation of Heat Capacity and Resistance to Cyclic Oxidation of Nickel Superalloys Journal title Archives of Foundry Engineering Yearbook 2014 Numer No 3 Authors Binczyk, F. ; Przeliorz, R. ; Góral, M. ; Gradoń, P. ; Mikuszewski, T. Keywords Foundry technology ; Nickel superalloys ; Heat resistance ; DSC calorimeter ; Heat capacity Divisions of PAS Nauki Techniczne Publisher The Katowice Branch of the Polish Academy of Sciences Date 2014 Type Artykuły / Articles Identifier DOI: 10.2478/afe-2014-0064 ; ISSN 2299-2944