Details

Title

Expert System for Analysis of Casting Defects - ESVOD

Journal title

Archives of Foundry Engineering

Yearbook

2015

Numer

No 1

Authors

Keywords

Expert system ; Identification of casting defects

Divisions of PAS

Nauki Techniczne

Publisher

The Katowice Branch of the Polish Academy of Sciences

Date

2015[2015.01.01 AD - 2015.12.31 AD]

Type

Artykuły / Articles

Identifier

DOI: 10.1515/afe-2015-0004 ; ISSN 2299-2944

Source

Archives of Foundry Engineering; 2015; No 1
×