Details Details PDF BIBTEX RIS Title Durability of MAR-247 and IN-713C Nickel Superalloys under Cyclic Creep Conditions Journal title Archives of Foundry Engineering Yearbook 2015 Issue No 4 Authors Cieśla, M. ; Junak, G. ; Gradoń, P. ; Binczyk, F. ; Mańka, M. Keywords Nickel superalloys ; Macrostructure modification ; Heat treatment ; Low-cycle fatigue ; Cyclic creep Divisions of PAS Nauki Techniczne Publisher The Katowice Branch of the Polish Academy of Sciences Date 2015[2015.01.01 AD - 2015.12.31 AD] Type Artykuły / Articles Identifier DOI: 10.1515/afe-2015-0071 Source Archives of Foundry Engineering; 2015; No 4