Application of X-Ray Microtomography and Optical Microscopy to Determine the Microstructure of Concrete Penetrated by Carbon Dioxide/ Zastosowanie Mikrotomografii Komputerowej I Mikroskopii Optycznej Do Oceny Mikrostruktury Betonów Poddanych Działaniu Co2

Journal title

Archives of Metallurgy and Materials

Yearbook

2014

Numer

No 4 December

Authors

Divisions of PAS

Nauki Techniczne

Publisher

Institute of Metallurgy and Materials Science of Polish Academy of Sciences ; Commitee on Metallurgy of Polish Academy of Sciences

Date

2014

Identifier

DOI: 10.2478/amm-2014-0245 ; ISSN 1733-3490
×