Influence of Modification and Casting Technology on Structure of IN-713C Superalloy Castings

Journal title

Archives of Foundry Engineering

Yearbook

2016

Issue

No 3

Authors

Keywords

Innovative casting materials and technologies ; Nickel alloy IN-713C ; Surface and volume modification ; Cobalt aluminate ; Macrostructure

Divisions of PAS

Nauki Techniczne

Publisher

The Katowice Branch of the Polish Academy of Sciences

Date

2016

Type

Artykuły / Articles

Identifier

DOI: 10.1515/afe-2016-0040

Source

Archives of Foundry Engineering; 2016; No 3

References

Binczyk (2010), Mechanical properties and creep resistance behaviour of IN - alloy castings of Foundry ISSN, Archives Engineering, 10, 713. ; Binczyk (2011), Ceramic filters for bulk inoculation of nickel alloy castings of Foundry special ISSN, Archives Engineering, 11, 29. ; Liu (2005), Grain refinement of superalloy by addition of refineries : cast structure and refinement mechanisms Science and, Materials Engineering, 4169. ; Binczyk (2011), Effect of technological parameters on structure of castings made from IN - nickel alloy of Foundry ISSN, Archives Engineering, 11, 713. ; Binczyk (2011), Modification of the macrostructure of nickel superalloys with cobalt nanoparticles ISSN, Composites, 1. ; Xiong (2001), Grain refinement of superalloys by the addition of refiners and Technology of Advanced Materials, Science, 4169. ; Pucka (1984), Preparing technology of gas turbine blades with adjustable grain size ( in Polish ), Materials Engineering, 4, 115. ; Binczyk (2010), Effect of modification on the mechanical properties of IN - alloy of Foundry ISSN, Archives Engineering, 10, 713. ; Binczyk (2010), Effect of repeated remelting on the chemical composition and structure of nickel alloys of Foundry special ISNN, Archives Engineering, 10, 189. ; Zielińska (2008), Effect of modification on microstructure and mechanical properties of cobalt casting superalloy of Metallurgy and Materials, Archives, 53, 887.
×