Details

Title

Study of Flow Softening Mechanisms of a Nickel-Based Superalloy With Δ Phase

Journal title

Archives of Metallurgy and Materials

Yearbook

2016

Issue

No 3 September

Authors

Divisions of PAS

Nauki Techniczne

Publisher

Institute of Metallurgy and Materials Science of Polish Academy of Sciences ; Committee of Materials Engineering and Metallurgy of Polish Academy of Sciences

Date

2016

Identifier

DOI: 10.1515/amm-2016-0251 ; ISSN 1733-3490

Source

Archives of Metallurgy and Materials; 2016; No 3 September

References

Lin (2014), Comput Mater Sci, 83, 282, doi.org/10.1016/j.commatsci.2013.11.003 ; Lin (2016), Mater Des, 97, 13. ; Quan (2013), Mater Res, 16, 1092, doi.org/10.1590/S1516-14392013005000091 ; Farabi (2015), Mater Sci Eng, 641. ; Zhang (2014), Mater Sci, 29, 2799. ; Abbasi (2012), Mater Sci Eng, 552. ; Souza (2015), Mater Sci Eng, 648. ; Samantaray (null), Mater Sci Eng, 5982014. ; Azarbarmas (2016), Mater Des, 94, 28. ; Samantaray (2011), Mater Sci Eng, 528. ; Quan (2015), High Temp Mater Process, 3, 4. ; Wen (2015), Mater Sci Eng, 620. ; Cheng (2014), Mater Sci Eng, 606. ; Bhattacharya (2012), Mater, 67. ; Sarkar (2006), Mater Sci Eng, 421. ; Lin (2014), Mater Des, 59, 115, doi.org/10.1016/j.matdes.2014.02.041 ; Zhang (2015), Mater Sci, 30, 1029. ; Lin (2011), Mater Des, 32, 1733, doi.org/10.1016/j.matdes.2010.11.048 ; Krawczyk (2012), Arch Metall Mater, 57593. ; Dadras (1981), Metall Trans A, 12, 1867, doi.org/10.1007/BF02643797 ; Li (2015), Mater Sci Eng, 628. ; Yang (2015), Mater Des, 84133. ; Li (2015), Mater Eng Perform, 24, 3539, doi.org/10.1007/s11665-015-1640-9 ; Żaba (2015), Arch Metall Mater, 60, 2637. ; Toan (2014), High Temp Mater Process, 33, 499. ; Lin (2016), Trans Nonferrous Met Soc China, 26, 2107. ; Liu (2014), Mater Des, 63, 829, doi.org/10.1016/j.matdes.2014.06.063 ; Mehtonen (2013), Mater Sci Eng, 571. ; Abbasi (2015), Mater Sci Eng, 639. ; Huda (2014), Arch Metall Mater, 59, 847. ; Gu (2015), Mater Eng Perform, 24, 1790, doi.org/10.1007/s11665-015-1460-y ; Nowotnik (2015), Arch Metall Mater, 60, 1079. ; Trimble (2015), Mater Des, 76, 150, doi.org/10.1016/j.matdes.2015.03.062 ; Zhang (2015), J Mech Sci, 98, 195, doi.org/10.1016/j.ijmecsci.2015.04.015 ; Zuo (2015), Prog Nat Sci Mater Int, 25, 66, doi.org/10.1016/j.pnsc.2015.01.007 ; Lin (2015), Mater Res, 30, 3784, doi.org/10.1557/jmr.2015.368 ; Lin (null), Mater Des Mater Des, 99, 107. ; Gao (2014), Mater Int, 20, 939, doi.org/10.1007/s12540-014-5020-z ; Chen (2015), Mater Des, 77, 41, doi.org/10.1016/j.matdes.2015.04.004 ; Lin (2014), Mater Sci Eng, 598. ; Miller (1999), Mater, 40, 1387. ; Liang (2013), Mater Sci Eng, 570. ; Lin (2015), and, Mater Eng Perform, 24, 23527. ; Kumar (2015), Mater Sci, 50, 6444, doi.org/10.1007/s10853-015-9200-0 ; Sołek (2015), Acta Metall Sinica, 28, 22, doi.org/10.1007/s40195-014-0150-3 ; Chen (2015), Mater Sci Eng, 642. ; Liu (2015), Study of dynamic recrystallization in a Ni - based superalloy by experiments and cellular automaton model, Mater Sci Eng, 626. ; Ye (2015), Iron Steel Res Int, 22, 752, doi.org/10.1016/S1006-706X(15)30068-6 ; Rakhshkhorshid (2015), J Manuf Technol, 77.
×