Details

Title

Effect of Process Control Agent on the Microstructure of Ni-Based ODS Superalloy Produced by Mechanical Alloying and Sintering

Journal title

Archives of Metallurgy and Materials

Yearbook

2019

Volume

vol. 64

Numer

No 3

Authors

Keywords

Ni-based superalloy ; Process control agents ; Mechanical alloying ; spark plasma sintering ; microstructure

Divisions of PAS

Nauki Techniczne

Coverage

949-952

Publisher

Institute of Metallurgy and Materials Science of Polish Academy of Sciences ; Commitee on Metallurgy of Polish Academy of Sciences

Date

2019.09.03

Type

Artykuły / Articles

Identifier

DOI: 10.24425/amm.2019.129478 ; ISSN 1733-3490

Source

Archives of Metallurgy and Materials; 2019; vol. 64; No 3; 949-952
×