Szczegóły

Tytuł artykułu

Microscale interpretation of tribological phenomena in Ti/TiN soft-hard multilayer coatings on soft austenite steel substrates

Tytuł czasopisma

Bulletin of the Polish Academy of Sciences Technical Sciences

Rocznik

2011

Wolumin

59

Numer

No 3

Autorzy

Wydział PAN

Nauki Techniczne

Zakres

343-355

Data

2011

Identyfikator

DOI: 10.2478/v10175-011-0042-x ; ISSN 2300-1917

Źródło

Bulletin of the Polish Academy of Sciences: Technical Sciences; 2011; 59; No 3; 343-355

Referencje

Holleck H. (1995), Multilayer PVD coatings for wear protection, Surf. Coat. Technol, 76-77, 328, doi.org/10.1016/0257-8972(95)02555-3 ; Nordin M. (1998), Mechanical and tribological properties of multilayered PVD TiN/CrN, TiN/MoN, TiN/NbN and TiN/TaN coatings on cemented carbide, Surf. Coat. Technol, 106, 234, doi.org/10.1016/S0257-8972(98)00544-1 ; Voevodin A. (1996), Multilayer composite ceramic- metal- DLC coatings for sliding wear applications, Tribol. Int, 29, 559, doi.org/10.1016/0301-679X(95)00121-J ; Stueber M. (2009), Concepts for the design of advanced nanoscale PVD multilayer protective thin films, J. Alloys and Compounds, 483, 321, doi.org/10.1016/j.jallcom.2008.08.133 ; Martinez E. (2003), Nanoindentation stress-strain curves as a method for thin-film complete mechanical characterization: application to nanometric CrN/Cr multilayer coatings, Appl. Phys, A 77, 419. ; Smolik J. (1999), Effect of interlayer composition on the tribological properties of TiC/Ti(C<sub>x</sub>, N<sub>1 - x</sub>)/TiN anti-abrasive multi-layer coatings, Vacuum, 55, 147, doi.org/10.1016/S0042-207X(99)00141-4 ; Su Y. (1998), Optimum multilayer TiN-TiCN coatings for wear resistance and actual application, Wear, 223, 119, doi.org/10.1016/S0043-1648(98)00276-2 ; Dück N. (2001), Ti/TiN multilayer coatings, deposition technique, characterization and mechanical properties, Surf. Coat. Technol, 142-144, 579, doi.org/10.1016/S0257-8972(01)01171-9 ; Labdi S. (1996), Elaboration and characterization of Ti and TiN thin films and Ti/TiN multilayers for hard coating applications, Thin Solid Films, 275, 213, doi.org/10.1016/0040-6090(95)07046-X ; Nordin M. (1999), Mechanical and tribological properties of multilayered PVD TiNrCrN, Wear, 232, 221, doi.org/10.1016/S0043-1648(99)00149-0 ; Nordin M. (1999), Wear resistance of multilayered PVD TiN/TaN on HSS, Surf. Coat. Technol, 120-121, 528, doi.org/10.1016/S0257-8972(99)00493-4 ; Smolik J. (1999), Investigation of adhesion between component layers of a multi-layer coating TiC/Ti(C<sub>x</sub>, N<sub>1 - x</sub>)/TiN by the scratch-test method, Vacuum, 55, 45, doi.org/10.1016/S0042-207X(99)00122-0 ; Bromark M. (1997), Wear of PVD Ti/TiN multilayer coatings, Surf. Coat. Technol, 90, 217, doi.org/10.1016/S0257-8972(96)03141-6 ; Leyland A. (1994), Thick Ti/TiN multilayered coatings for abrasive and erosive wear resistance, Surf. Coat. Technol, 70, 19, doi.org/10.1016/0257-8972(94)90069-8 ; Matthews A. (1994), Engineering applications for diamond-like carbon, Diamond Relat. Mater, 3, 902, doi.org/10.1016/0925-9635(94)90297-6 ; Holmberg K. (1998), Coatings tribology-contact mechanics and surface design, Tribol. Int, 31, 1-3, 107, doi.org/10.1016/S0301-679X(98)00013-9 ; Matthews A. (2001), Modelling the deformation behaviour of multilayer coatings, Tribology Letters, 11, 103, doi.org/10.1023/A:1016667932251 ; Kim G. (2003), Effects of the thickness of Ti buffer layer on the mechanical properties of TiN coatings, Surf. Coat. Technol, 171, 83, doi.org/10.1016/S0257-8972(03)00243-3 ; Lackner J. (2007), Industrially-scaled room-temperature pulsed laser deposition of Ti-TiN multilayer coatings, J. Physics, Conf. Series, 59, 16, doi.org/10.1088/1742-6596/59/1/004 ; Farhat Z. (1997), Nanoindentation and friction studies on Ti-based nanolaminated films, Surf. Coat. Technol, 89, 24, doi.org/10.1016/S0257-8972(96)02939-8 ; Zhang S. (2007), Thin Films and Coatings. ; Leyland A. (1994), Thick Ti/TiN multilayered coatings for abrasive and erosive wear resistance, Surf. Coat. Technol, 70, 19. ; Holmberg K. (1998), Coatings tribology - contact mechanisms and surface design, Tribol. Intern, 31, 107. ; Chan K. (1993), Cracking and stress redistribution in ceramic layered composites, Mater. Sci. Eng, 167, 57, doi.org/10.1016/0921-5093(93)90337-E ; He M. (1994), Crack deflection at an interface between dissimilar elastic materials, role of residual stresses, Int. J. Solids. Struct, 31, 3443, doi.org/10.1016/0020-7683(94)90025-6 ; Lackner J. (2006), Industrially-scaled hybrid Pulsed Laser Deposition at Room Temperature. ; Oliver W. (1992), Piezoelectric nanoindentation, J. Materials Research, 7, 1564. ; Fischer-Cripps A. (2006), Critical review of analysis and interpretation of nanoindentation test data, Surface and Coatings Technology, 200, 4153, doi.org/10.1016/j.surfcoat.2005.03.018 ; Zhang X. (2007), Hertzian contact response of single-layer, functionally graded and sandwich coatings, Materials and Design, 28, 47, doi.org/10.1016/j.matdes.2005.06.018 ; Tilbrook M. (2007), Microstructural effects on indentation failure mechanisms in TiN coatings, finite element simulations, Acta Materialia, 55, 2489, doi.org/10.1016/j.actamat.2006.11.043 ; Vlachos D. (2001), 3-D modeling of nanoindentation experiment on a coating-substrate system, Computational Mechanics, 27, 138, doi.org/10.1007/s004660000222 ; Liu S. (2005), An extension of the Hertz theory for 2D coated components, Tribology Letters, 18, 505, doi.org/10.1007/s11249-005-3611-z ; Zhang X. (2007), Hertzian contact response of single-layer, functionally graded and sandwich coatings, Materials and Design, 28, 47. ; Pane I. (2005), Response to loading and stiffness of coated substrates indented by spheres, Surface and Coatings Technology, 200, 1761, doi.org/10.1016/j.surfcoat.2005.08.050 ; Kot M. (2010), Deformations and fracture of coating-substrate systems under contact load, Tribologia, 231, 125. ; Lawn B. (2004), Fracture and deformation in brittle solids, a perspective on the issue of scale, J. Mater. Res, 19, 22, doi.org/10.1557/jmr.2004.19.1.22 ; Lawn B. (1975), Indentation fracture: principles and applications, J. Mater. Sci, 10, 1049, doi.org/10.1007/BF00823224 ; Lawn B. (2002), Overview: damage in brittle layer structures from concentrated loads, J. Mater. Res, 17, 3019, doi.org/10.1557/JMR.2002.0440 ; Chai H. (1999), Fracture modes in brittle coatings with large interlayer modulus mismatch, J. Mater. Res, 14, 3805. ; Weppelmann E. (1996), Investigation of the stresses and stress intensity factors responsible for fracture of thin protective films during ultra-micro indentation tests with spherical indenters, Thin Solid Films, 286, 111, doi.org/10.1016/S0040-6090(95)08525-4 ; Anderson R. (1998), Indentation response and cracking of sub-micron silica films on a polymeric substrate, Eng. Fract. Mech, 61, 93, doi.org/10.1016/S0013-7944(98)00057-5 ; Chai H. (2000), Role of adhesive interlayer I transverse fracture of brittle layer structures, J. Mater. Res, 15, 1653. ; Leyland A. (2000), On the significance of the H/E ratio in wear control: a nanocomposite coating approach to optimised tribological behavior, Wear, 246, 1, doi.org/10.1016/S0043-1648(00)00488-9 ; Matthews A. (2000), Developments in PVD tribological coatings, null, 1. ; Holmberg K. (1996), Coatings Tribology, Properties, Techniques and Applications, Surface Engineering. ; Holmberg K. (1994), Coatings tribology: a concept, critical aspects and future directions, Thin Solid Films, 253, 173, doi.org/10.1016/0040-6090(94)90315-8 ; Matthews A. (1998), Design aspects for advanced tribological surface coatings, Surf. Coat. Technol, 100-101, 1, doi.org/10.1016/S0257-8972(97)00578-1 ; Michler J. (2001), Analysis of coating fracture and substrate plasticity induced by spherical indentors: diamond and diamond-like carbon layers on steel substrates, Thin Solid Films, 381, 119, doi.org/10.1016/S0040-6090(00)01340-7 ; Bunshah R. (2001), Handbook of Hard Coating. ; Gwidon S. (2005), Wear - Materials, Mechanisms and Practise. ; Lackner J. (2010), Mechanisms for self-assembling topography formation in low-temperature vacuum deposition of inorganic coatings on polymer surfaces, Bull. Pol. Ac.: Tech, 58, 281. ; Lousa A. (2001), Multilayered chromium/chromium nitride coatings for use in pressure die-casting, Surface and Coatings Technology, 146-147, 268, doi.org/10.1016/S0257-8972(01)01476-1 ; Romero J. (2004), Period dependence of hardness and microstructure on nanometric Cr/CrN multilayers, Surface and Coatings Technology, 188-189, 338, doi.org/10.1016/j.surfcoat.2004.08.058 ; Maille L. (2004), A mechanical study of W-N/W multilayers, Surface and Coatings Technology, 180-181, 483, doi.org/10.1016/j.surfcoat.2003.10.092 ; Kim S. (2004), Analysis of interfacial strengthening from composite hardness of TiN/VN and TiN/NbN multilayer hard coatings, Surface and Coatings Technology, 187, 47, doi.org/10.1016/j.surfcoat.2004.01.011 ; Abadias G. (2006), Nanoindentation hardness and structure of ion beam sputtered TiN, W and TiN/W multilayer hard coatings, Surface and Coatings Technology, 200, 6538, doi.org/10.1016/j.surfcoat.2005.11.053 ; Berger M. (1999), The multilayer effect in abrasion - optimising the combination of hard and tough phases, Surface and Coatings Technology, 116-119, 1138, doi.org/10.1016/S0257-8972(99)00151-6 ; Kot M. (2008), Effect of bilayer period on properties of Cr/CrN multilayer coatings produced by laser ablation, Surface and Coatings Technology, 202, 3501, doi.org/10.1016/j.surfcoat.2007.12.036 ; Tien S. (2006), Effect of heat treatment on mechanical properties and microstructure of CrN/AlN multilayer coatings, Thin Solid Films, 494, 173, doi.org/10.1016/j.tsf.2005.08.198 ; Kim G. (2003), Synthesis of CrN/AlN superlattice coatings using closed-field unbalanced magnetron sputtering process, Surf. Coat. Technol, 171, 91, doi.org/10.1016/S0257-8972(03)00244-5 ; Dück A. (2001), Ti/TiN multilayer coatings: deposition technique, characterization and mechanical properties, Surf. Coat. Technol, 142-144, 579. ; Hall E. (1951), The deformation and ageing of mild steel, 1st Proc. Physics Society III Discussion of Results B, 64, 747, doi.org/10.1088/0370-1301/64/9/303 ; Lehoczky S. (1978), Retardation of dislocation generation and motion in thin-layered metal laminates, Review Letter, 41, 1814, doi.org/10.1103/PhysRevLett.41.1814 ; Vieira M. (1999), The influence of ductile interlayers on the mechanical performance of tungsten nitride coatings, J. Materials Processing Technology, 92-93, 156, doi.org/10.1016/S0924-0136(99)00235-6 ; Bemporad E. (2006), High thickness Ti/TiN multilayer thin coatings for wear resistant applications, Surface and Coatings Technology, 201, 2155, doi.org/10.1016/j.surfcoat.2006.03.042 ; Leyland A. (2004), Design criteria for wear-resistant nanostructured and glassy-metal coatings, Surf. Coat. Technol, 177-178, 317, doi.org/10.1016/j.surfcoat.2003.09.011 ; Tsui T. (1995), Nanoindentation and nanoscratching of hard carbon coatings for magnetic disks mater, Res. Soc. Symp. Proc, 383, 447, doi.org/10.1557/PROC-383-447 ; Musil J. (2000), Hard and superhard nanocomposite coatings, Surface and Coatings Technology, 125, 322, doi.org/10.1016/S0257-8972(99)00586-1 ; Pei Y. (2006), Self-lubrication and wear behavior of TiC/a-C:H nanocomposite coatings, J. Appl. Phys, 100, 114309. ; Karimi A. (2002), Fracture mechanisms in nanoscale layered hard thin films, Thin Solid Films, 420-421, 275, doi.org/10.1016/S0040-6090(02)00944-6 ; Hutchinson J. (1992), Growth and configurational stability of circular, buckling-driven film delaminations, Acta Metall, 40, 295, doi.org/10.1016/0956-7151(92)90304-W ; Kot M. (2010), Analysis of the influence of sublayer thickness on the deformation mechanism and fracture of {Ti/TiN} multilayer, Tribology, 232, 181. ; Kot M. (2008), Deformation of coating-substrate systems under contact load, Tribology, 218, 285. ; Herbert E. (2001), On the measurement of stress-strain curves by spherical indentation, Thin Solid Films, 398-399, 331, doi.org/10.1016/S0040-6090(01)01439-0 ; Carvalho N. (2006), Deformation mechanisms in TiN/(Ti, Al)N multilayers under depth-sensing indentation, Acta Materialia, 54, 1857, doi.org/10.1016/j.actamat.2005.12.010 ; Oden M. (1997), Characterization of the induced plastic zone in a single crystal TiN(001) film by nanoindentation and transmission electron microscopy, J. Mater. Res, 12, 2134, doi.org/10.1557/JMR.1997.0286 ; Hayashi T. (2003), Multidimensional infrared signatures of intramolecular hydrogen-bonding in malonaldehyde, J. Phys. Chem, 1079, 113. ; Park J.-K. (2007), Improvement of hardness and toughness of TiAlN coating by nanoscale multilayered structurization with Si<sub>3</sub>N<sub>4</sub>, Plasma Process. Polym, 4, 902, doi.org/10.1002/ppap.200732202 ; Xie Z. (2008), Deformation mechanisms of TiN multilayer coatings alternated by ductile or stiff interlayers, Acta Materialia, 56, 852, doi.org/10.1016/j.actamat.2007.10.047 ; Ma K. (1995), Examination of mechanical properties and failure mechanisms of TiN and Ti-TiN multilayer coatings, Surf. Coat. Technol, 76-77, 297, doi.org/10.1016/0257-8972(95)02585-5 ; Hübler R. (1993), Ion beam mixing of Al-AlN multilayers for tribological and corrosion protection, Nuc. Inst. Met. Phy. Res. B, 80-81, 1415, doi.org/10.1016/0168-583X(93)90811-J ; Martinez E. (2003), Wear behavior of nanometric CrN/Cr multilayers, Surface and Coatings Technology, 163-164, 571, doi.org/10.1016/S0257-8972(02)00664-3
×