Details Details PDF BIBTEX RIS Title Functional Properties of Aluminide Layer Deposited on Inconel 713 LC Ni-based Superalloy in the CVD Process Właściwości Użytkowe Warstwy Aluminidkowej Wytworzonej W Procesie CVD Na Stopie Niklu Inconel 713 LC Journal title Archives of Metallurgy and Materials Yearbook 2011 Issue No 1 March Authors Yavorska, M. ; Sieniawski, J. ; Zielińska, M. Divisions of PAS Nauki Techniczne Publisher Institute of Metallurgy and Materials Science of Polish Academy of Sciences ; Committee of Materials Engineering and Metallurgy of Polish Academy of Sciences Identifier DOI: 10.2478/v10172-011-0022-z ; ISSN 1733-3490 Source Archives of Metallurgy and Materials; 2011; No 1 March