Search results

Number of results: 9
items per page: 25 50 75
Sort by:
Download PDF Download RIS Download Bibtex

Abstract

In this research, AA7068/Si3N4 composites were fabricated through stir casting with the attachment of ultrasonic treatment. The quenching medium and aging duration significantly influenced the hardness of Al alloy samples. Peak hardness was achieved after 12 h of artificial aging at the temperature of 140°C. The addition of nano Si3N4 significantly refined the microstructure of unreinforced AA7068. The dispersion of intermetallic compounds (MgZn2) and grain boundary discontinuation were noticed after the T-6 heat treatment. Ultimate tensile strength, yield strength, and hardness were improved by 70.95%, 76.19%, and 44.33%, respectively, with the addition of 1.5 weight % Si3N4 compared to as-cast alloy due to the combined effect of heat treatment, hall-Petch, Orowan, thermal miss match, load-bearing strengthening mechanisms and uniform dispersion of reinforcement. A reduction in percentage elongation was noticed due to composites’ brittle nature by the effect of ceramic Si3N4 particles’ inclusion. The fracture surfaces reveal ductile failure for alloy and mixed-mode failure in the case of composites.
Go to article

Authors and Affiliations

Ashish Kumar
1
ORCID: ORCID
Ravindra Singh Rana
1
Rajesh Purohit
1
Anurag Namdev
1

  1. Maulana Azad National Institute of Technology, Department of Mechanical Engineering, Bhopa l, Madhya Pradesh, India
Download PDF Download RIS Download Bibtex

Abstract

CMT-WAAM, an advanced manufacturing technology, garners significant attention due to its ability to fabricate intricate components efficiently. In this investigation, a 40-layered structure was manufactured from SS 316L using the CMT-WAAM process, with the utilization of optimized process parameters. This research involved the analysis of microstructure and mechanical properties, including microhardness, tensile testing, and fractography, for both WAAM and wrought SS 316L. The UTS of WAAM reached 592.31 MPa and YS of 276.46 MPa, outperforming the UTS of wrought 316L, which was 557.62 MPa, and YS of 284.35 MPa. The PE of WAAM was 59.85%, while for wrought 316L, it was 53.20%, indicating that wrought 316L demonstrated a higher ductility than the WAAM part. The microhardness profile of WAAM showed an average value of 238.14 HV, indicating a 28% increase compared to the MH of wrought 316L, which was measured at 192.37 HV. The microstructure of CMT-WAAM displays δ-ferrite and γ-austenite, along with skeletal and lathy ferrites, similar in wrought 316L. The fractography analysis of tensile specimens exhibited numerous dimples, indicating favorable ductility in the fabricated structure. Therefore, the findings indicate that the CMT-WAAM process meets industrial requirements.
Go to article

Authors and Affiliations

S. Kumar Jain
1
ORCID: ORCID
Q. Murtaza
1
ORCID: ORCID
P. Singh
1
ORCID: ORCID

  1. Delhi Technological University, Department of Mechanical Engineering, Delhi-110042 (India)
Download PDF Download RIS Download Bibtex

Abstract

The paper presents the susceptibility of AE44 magnesium alloy to electrochemical corrosion and stress corrosion cracking (SCC). The evaluation of the intensity of the interaction of the corrosive environment was carried out using the corrosion tests and the Slow Strain Rate Test (SSRT). Corrosion tests performed in 0.1 M Na2SO4 solution (immersion in solution and under cathodic polarization conditions) revealed that the layer of corrosion products was much thicker after immersion test. The results of SSRT showed that the AE44 alloy deformed in the solution was characterized by higher plasticity compared to the alloy deformed in the air after immersion in solution. Moreover, the fractures were characterized by different morphology. In the case of an alloy deformed in the solution under cathodic polarization many microcracks on the fracture were observed, which were not observed in the case of the alloy deformed in the air.

Go to article

Authors and Affiliations

M. Sozańska
A. Mościcki
B. Chmiela
Download PDF Download RIS Download Bibtex

Abstract

Cauchy paved the way for constructing models in concrete technology, and elsewhere. He determined the (nonflat) surface area in 3D by measuring random total projections. Analogously, he determined the length of a curved line in 2D by way of measuring the total projections. The paper will present the mathematical expressions, because in many branches of concrete technology, modelling is found based on such Cauchy concepts. These branches – fractography in compression, tension or shear, fibre reinforcement and permeability estimation – will briefly be mentioned to demonstrate this. It has been found that, for the discussed fields of engineering relevance, major model parameters for cementitious materials are similar to those developed by Cauchy in the 19th century. In the paper some previous investigations concerning fractography, fibre reinforcement and fracture roughness will be summarized but basically a new development on porosimetry will be presented. Particularly a new achievement of successful implementation of the methodology (also based on Cauchy) for optimizing permeability estimation will be discussed.

Go to article

Authors and Affiliations

P. Stroeven
M. Słowik
Download PDF Download RIS Download Bibtex

Abstract

The paper evaluates the causes related to the fatigue damage in a conveyor slide plate, exposed to high-frequency cyclic loads. The plate was made of 1.4301 acid-resistant steel. The fractography showed that the plate failure was caused by fatigue crack. A nonlinear analysis of plate deformation was conducted using the finite element method (FEA) in LS-Dyna software. The maximum normal stresses in the plate fracture were used in further analysis. A “fatigue limit” calculated initially using a FITNET procedure was above the maximum stress calculated using FEA. It indicates that the structural features of the plate were selected correctly. The experimental test results for 1.4301 acid-resistant steel were described using a probabilistic Weibull distribution model. Reliability was determined for the obtained S-N curve at 50% and 5% failure probability allowing for the selected coefficients (cycle asymmetry, roughness, variable load) and the history of cyclic loading. Cumulative damage was determined using the Palmgren-Miner hypothesis. The estimated fatigue life was similar to the actual value determined in the operating conditions for the S-N curve at 5% failure probability. For engineering calculations, the S-N curve at max. 5% failure probability is recommended.

Go to article

Authors and Affiliations

T. Tomaszewski
P. Strzelecki
M. Wachowski
ORCID: ORCID
M. Stopel
Download PDF Download RIS Download Bibtex

Abstract

There is growing interest in developing more advanced materials, as conventional materials are unable to meet the demands of the automotive, aerospace, and military industries. To meet the needs of these sectors, the use of advanced materials with superior properties, such as metal matrix composites, is essential. This paper discusses the evaluation of microstructural and mechanical properties of conventional eutectic EN AC-AlSi12CuNiMg aluminum alloy (AlSi12) and advanced composite based on EN AC-AlSi12CuNiMg alloy matrix with 10 wt% SiC particle reinforcement (AlSi12/10SiCp). The microstructure of these materials was investigated with the help of metallographic techniques, specifically using a light microscope (LM) and a scanning electron microscope (SEM). The results of the microstructural analysis show that the SiC particles are uniformly distributed in the matrix. The results of the mechanical tests indicate that the tensile properties and hardness of the AlSi12/10SiCp composite are significantly higher than those of the unreinforced eutectic alloy. For AlSi12/10SiCp composite, the tensile strength is 21% higher, the yield strength is 16% higher, the modulus of elasticity is 20% higher, and the hardness is 11% higher than unreinforced matrix alloy. However, the unreinforced AlSi12 alloy has a percentage elongation that is 16% higher than the composite material. This shows that the AlSi12/10SiCp composite has a lower ductility than the unreinforced AlSi12 alloy. The tensile specimens of the tested composite broke apart in a brittle manner with no discernible neck development, in contrast to the matrix specimens, which broke apart in a ductile manner with very little discernible neck formation.
Go to article

Bibliography


[1] Rashnoo, K., Sharifi, M. J., Azadi, M. & Azadi, M. (2020). Influences of reinforcement and displacement rate on microstructure, mechanical properties and fracture behaviors of cylinder-head aluminum alloy. Materials Chemistry and Physics. 255, 123441, 1-13. DOI: 10.1016/j.matchemphys.2020.123441.

[2] Azadi, M., Winter, G., Farrahi, G.H. & Eichlseder, W. (2015). Comparison between isothermal and non-isothermal fatigue behavior in a cast aluminum-silicon-magnesium alloy. Strength of Materials. 47(6), 840-848. DOI: 10.1007/s11223-015-9721-4.

[3] Aybarc, U., Dispinar, D. & Seydibeyoglu, M.O. (2018). Aluminum metal matrix composites with SiC, Al 2 O 3 and graphene–review. Archives of Foundry Engineering. 18(2), 5-10. DOI: 10.24425/122493.

[4] Arora, A., Astarita, A., Boccarusso, L. & Mahesh, V.P. (2016). Experimental characterization of metal matrix composite with aluminium matrix and molybdenum powders as reinforcement. Procedia Engineering. 167, 245-251. DOI: 10.1016/j.proeng.2016.11.694.

[5] Farokhpour, M., Parast, M.S.A. & Azadi, M. (2022). Evaluation of hardness and microstructural features in piston aluminum-silicon alloys after different ageing heat treatments. Results in Materials. 16, 100323, 1-11. DOI: 10.2139/ssrn.4162353.

[6] Sirata, G.G., Wacławiak, K. & Dyzia, M. (2022). Mechanical and Microstructural Characterization of aluminium alloy, EN AC-Al Si12CuNiMg. Archives of Foundry Engineering. 22(3), 34-40. DOI: 10.24425/afe.2022.140234.

[7] Kurzawa, A. & Kaczmar, J.W. (2017). Bending strength of EN AC-44200–Al2O3 composites at elevated temperatures. Archives of Foundry Engineering. 17(1), 103-108. DOI: 10.1515/afe-2017-0019.

[8] Lijay, K.J., Selvam, J.D.R., Dinaharan, I. & Vijay, S.J. (2016). Microstructure and mechanical properties characterization of AA6061/TiC aluminum matrix composites synthesized by in situ reaction of silicon carbide and potassium fluotitanate. Transactions of Nonferrous Metals Society of China. 26(7), 1791-1800. DOI: 10.1016/S1003-6326(16)64255-3.

[9] Lakshmipathy, J. & Kulendran, B. (2014). Reciprocating wear behavior of 7075Al/SiC in comparison with 6061Al/Al2O3 composites. International Journal of Refractory Metals and Hard Materials. 46, 137-144. DOI: 10.1016/j.ijrmhm.2014.06.007.

[10] Jayashree, P.K., Gowrishankar, M.C., Sharma, S., Shetty, R., Hiremath, P. & Shettar, M. (2021). The effect of SiC content in aluminum-based metal matrix composites on the microstructure and mechanical properties of welded joints. Journal of Materials Research and Technology. 12, 2325-2339. DOI: 10.1016/j.jmrt.2021.04.015.

[11] Dolata-Grosz, A., Dyzia, M., Śleziona, J. & Wieczorek, J. (2007). Composites applied for pistons. Archives of Foundry Engineering. 7(1), 37-40. ISSN (1897-3310).

[12] Moćko, W. & Kowalewski, Z.L. (2011). Mechanical properties of A359/SiCp metal matrix composites at wide range of strain rates. Applied Mechanics and Materials. 82, 166-171. https://doi.org/10.4028/www.scientific.net/ AMM.82.166.

[13] Dolata, A.J. & Dyzia, M. (2014). Effect of Chemical Composition of the Matrix on AlSi/SiC p+ C p Composite Structure. Archives of Foundry Engineering. 14(1), 135-138. ISSN (1897-3310).

[14] Wysocki, J., Grabian, J. & Przetakiewicz, W. (2007). Continuous drive friction welding of cast AlSi/SiC (p) metal matrix composites. Archives of Foundry Engineering. 7(1), 47-52. ISSN (1897-3310).

[15] Li, R., Pan, Z., Zeng, Q. & Xiaoli, Y. (2022). Influence of the interface of carbon nanotube-reinforced aluminum matrix composites on the mechanical properties–a review. Archives of Foundry Engineering. 22(1), 23-36. DOI: 10.24425/afe.2022.140213.

[16] Dolata, A.J., Mróz, M., Dyzia, M. & Jacek-Burek, M. (2020). Scratch testing of AlSi12/SiCp composite layer with high share of reinforcing phase formed in the centrifugal casting process. Materials. 13(7), 1685, 1-17. DOI: 10.3390/ma13071685.

[17] Pawar, P.B., & Utpat, A.A. (2014). Development of aluminium based silicon carbide particulate metal matrix composite for spur gear. Procedia Materials Science, 6, 1150-1156. DOI:10.1016/j.mspro.2014.07.187.

[18] Miracle, D.B. (2005). Metal matrix composites–from science to technological significance. Composites science and technology, 65(15-16), 2526-2540. DOI: 10.1016/j.compscitech.2005.05.027.

[19] Dyzia, M. (2017). Aluminum matrix composite (AlSi7Mg2Sr0. 03/SiCp) pistons obtained by mechanical mixing method. Materials. 11(1), 42, 1-14. DOI: 10.3390/ma11010042.

[20] Sahoo, B.P.,& Das, D. (2019). Critical review on liquid state processing of aluminium based metal matrix nano-composites. Materials Today: Proceedings. 19, 493-500. DOI: 10.1016/j.matpr.2019.07.642.

[21] Yar, A.A., Montazerian, M., Abdizadeh, H. & Baharvandi, H.R. (2009). Microstructure and mechanical properties of aluminum alloy matrix composite reinforced with nano-particle MgO. Journal of alloys and Compounds. 484(1-2), 400-404. DOI: 10.1016/j.jallcom.2009.04.117.

[22] Kumar, B.A. & Murugan, N. (2012). Metallurgical and mechanical characterization of stir cast AA6061-T6–AlNp composite. Materials & Design. 40, 52-58. DOI: 10.1016/j.matdes.2012.03.038.

[23] Peng, L.M., Han, K.S., Cao, J.W. & Noda, K. (2003). Fabrication and mechanical properties of high-volume-fraction Si3N4-Al-based composites by squeeze infiltration casting. Journal of Materials Science Letters. 22(4), 279-282. DOI: 1022356413756.

[24] Rajan, T.P.D., Pillai, R.M., & Pai, B.C. (2008). Centrifugal casting of functionally graded aluminium matrix composite components. International Journal of Cast Metals Research. 21(1-4), 214-218. DOI: 10.1179/136404608X361972.

[25] Chen, H.S., Wang, W.X., Li, Y.L., Zhang, P., Nie, H.H. & Wu, Q.C. (2015). The design, microstructure and tensile properties of B4C particulate reinforced 6061Al neutron absorber composites. Journal of Alloys and Compounds. 632, 23-29. DOI: 10.1016/j.jallcom.2015.01.048.

[26] Rohatgi, P.K. & Schultz, B. (2007). Lightweight metal matrix nanocomposites–stretching the boundaries of metals. Material Matters. 2(4), 16-20.

[27] Torralba, J.D., Da Costa, C.E. & Velasco, F. (2003). P/M aluminum matrix composites: an overview. Journal of Materials Processing Technology. 133(1-2), 203-206. DOI: 10.1016/S0924-0136(02)00234-0.

[28] Suryanarayana, C. & Al-Aqeeli, N. (2013). Mechanically alloyed nanocomposites. Progress in Materials Science. 58(4), 383-502. DOI: 10.1016/j.pmatsci.2012.10.001.

[29] Taha, M.A. (2001). Practicalization of cast metal matrix composites (MMCCs). Materials & Design. 22(6), 431-441. DOI: 10.1016/S0261-3069(00)00077-7.

[30] Maurya, M., Maurya, N.K. & Bajpai, V. (2019). Effect of SiC reinforced particle parameters in the development of aluminium based metal matrix composite. Joint Journal of Novel Carbon Resource Sciences & Green Asia Strategy. 06(03), 200-206. DOI: 10.5109/2349295.

[31] Sharma, P., Sharma, S. & Khanduja, D. (2015). A study on microstructure of aluminium matrix composites. Journal of Asian Ceramic Societies. 3(3), 240-244. DOI: 10.1016/j.jascer.2015.04.001.

[32] Chandra, D., Chauhan, N. R. & Rajesha, S. (2020). Hardness and toughness evaluation of developed Al metal matrix composite using stir casting method. Materials Today: Proceedings. 25, 872-876. DOI: 10.1016/j.matpr.2019.12.026.

[33] Kaviyarasan, K., Kumar, J.P., Anandh, S.K., Sivavishnu, M. & Gokul, S. (2020). Comparison of mechanical properties of Al6063 alloy with ceramic particles. Materials Today: Proceedings. 22, 3067-3074. DOI: 10.1016/j.matpr.2020.03.442.

[34] Subramanya Reddy, P., Kesavan, R. & Vijaya Ramnath, B. (2017). Evaluation of mechanical properties of aluminum alloy (Al2024) reinforced with silicon carbide (SiC) metal matrix Composites. Solid State Phenomena. 263, 184-188. DOI: 10.4028/www.scientific.net/SSP.263.184.

[35] Nair, S.V., Tien, J.K. & Bates, R.C. (1985). SiC-reinforced aluminium metal matrix composites. International Metals Reviews. 30(1), 275-290. https://doi.org/10.1179/ imtr.1985.30.1.275.

[36] Ozben, T., Kilickap, E. & Cakır, O. (2008). Investigation of mechanical and machinability properties of SiC particle reinforced Al-MMC. Journal of Materials Processing Technology. 198(1-3), 220-225. DOI: 10.1016/j.jmatprotec.2007.06.082.

[37] Ozden, S., Ekici, R. & Nair, F. (2007). Investigation of impact behaviour of aluminium based SiC particle reinforced metal–matrix composites. Composites Part A: Applied Science and Manufacturing. 38(2), 484-494. DOI: 10.1016/j.compositesa.2006.02.026.

[38] Shuvho, M.B.A., Chowdhury, M.A., Kchaou, M., Roy, B. K., Rahman, A. & Islam, M.A. (2020). Surface characterization and mechanical behavior of aluminum based metal matrix composite reinforced with nano Al2O3, SiC, TiO2 particles. Chemical Data Collections. 28, 100442. DOI: 10.1016/j.cdc.2020.100442.

[39] Peng, Z. & Fuguo, L. (2010). Effects of particle clustering on the flow behavior of SiC particle reinforced Al metal matrix composites. Rare Metal Materials and Engineering. 39(9), 1525-1531. DOI: 10.1016/S1875-5372(10)60123-3.

[40] Kurzawa, A. & Kaczmar, J.W. (2017). Impact strength of composite materials based on EN AC-44200 matrix reinforced with Al2O3 particles. Archives of Foundry Engineering. 17(3), 73-78. DOI: 10.1515/afe-2017-0094.

[41] Azadi, M., Bahmanabadi, H., Gruen, F. & Winter, G. (2020). Evaluation of tensile and low-cycle fatigue properties at elevated temperatures in piston aluminum-silicon alloys with and without nano-clay-particles and heat treatment. Materials Science and Engineering: A. 788, 139497, 1-16. DOI: 10.1016/j.msea.2020.139497.

[42] Li, Y., Yang, Y., Wu, Y., Wang, L. & Liu, X. (2010). Quantitative comparison of three Ni-containing phases to the elevated-temperature properties of Al–Si piston alloys. Materials Science and Engineering: A. 527(26), 7132-7137. DOI: 10.1016/j.msea.2010.07.073.

[43] Dolata, A.J., Dyzia, M. & Boczkal, S. (2016). Structure of interface between matrix alloy and reinforcement particles in Al/SiCp+ Cgp hybrid composites. Materials Today: Proceedings. 3(2), 235-239. DOI: 10.1016/j.matpr.2016.01.063.

[44] Keshavamurthy, R., Mageri, S., Raj, G., Naveenkumar, B., Kadakol, P.M. & Vasu, K. (2013). Microstructure and mechanical properties of Al7075-TiB2 in-situ composite. Research Journal of Material Sciences. 1(10), 6-10. ISSN 2320- 6055.

[45] Moustafa, S.F. (1995). Wear and wear mechanisms of Al-22% Si/A12O3f composite. Wear. 185(1-2), 189-195. DOI: 10.1016/0043-1648(95)06607-1.

Go to article

Authors and Affiliations

G.G. Sirata
1
ORCID: ORCID
K. Wacławiak
1
ORCID: ORCID
A.J. Dolata
1

  1. Department of Materials Technologies, Faculty of Materials Engineering, Silesian University of Technology, Krasińskiego 8, 40-019 Katowice, Poland
Download PDF Download RIS Download Bibtex

Abstract

The primary goal of the research work is, to employ a novel alloy as the skin material of the spaceship as a replacement for Al2024-T3. As a part of this task, a twin rolled Al-Cu wrought alloy, Al2016, was received after being age hardened to T6 condition. This article focuses on the fatigue properties and post-fracture analysis of the Al2016-T6 Alloy. Specimens were prepared according to ASTM E606 standards, and subjected to a rotating-bending fatigue testing machine. As a result, the fatigue property of the Al2016-T6 alloy was determined by Wohler’s curve method, fatigue life prediction through the Basquin Equation, estimation of fatigue strength for infinite fatigue life using the Kohout-Věchet model, and fatigue fractography observations via SEM images. The mode of fracture, the origin of fracture and its mechanism, and the morphology of fractured surfaces were reported after investigation. The outcomes of this alloy were compared and discussed with the properties of the existing skin material of the spacecraft, Al2024-T3.
Go to article

Authors and Affiliations

R. Arivumani
1 2
ORCID: ORCID
P. Ilamathi
1
ORCID: ORCID
K. Balamurugan
3
ORCID: ORCID

  1. Department of Production Engineering, Government College of Technology, Coimbatore, 641013, Tamilnadu, India
  2. Department of Mechanical Engineering, KIT-Kalaignar Karunanidhi Institute of Technology, Coimbatore, 641402, India
  3. Department of Mechanical Engineering, Governme nt College of Engineering, Erode, 638316, Tamilnadu, India
Download PDF Download RIS Download Bibtex

Abstract

Fractography of stress corrosion cracking (SCC) of 20% cold worked Type 304 H stainless steel containing δ-ferrite was studied using a compact tension (CT) specimen in oxidizing primary water with a scanning electron microscope (SEM) and electron back scattered diffraction (EBSD). The stress corrosion crack propagated mostly in transgranular stress corrosion cracking (TGSCC) mode and sometimes in intergranular stress corrosion cracking (IGSCC) mode. TGSCC paths were along the {111} plane with both high resolved shear stress and high resolved tensile stress. IGSCC preferentially propagated along the grain boundary perpendicular to the loading axis. The findings in this work suggest that TGSCC proceeds through formation of a weakening zone at the head of the crack tip by interaction of slip and corrosion and then cracking of the weakened zone by tensile stress.
Go to article

Authors and Affiliations

Hong-Pyo Kim
1
ORCID: ORCID
Jong-Yeon Lee
1
ORCID: ORCID
Sung-Hwan Cho
1
ORCID: ORCID
Min-Jae Choi
1
ORCID: ORCID
Sung-Woo Kim
1
ORCID: ORCID
Hyung-Ha Jin
1
ORCID: ORCID
Dong-Jin Kim
1
ORCID: ORCID
Seoung-Sik Hwang
1
ORCID: ORCID
Yun-Soo Lim
1
ORCID: ORCID

  1. Korea Atomic Energy Rese arch Institute , Materials Safety Research Division, 989-111 Daedeok-daero, Yuseong-gu, Daejeon, 305-353, Republic of Korea
Download PDF Download RIS Download Bibtex

Abstract

An arc is used as a heat source in the manufacturing process known as wire arc additive manufacturing (WAAM), which uses layer-by-layer cladding to fuse wire. In the current work, Wire Arc Additive Manufacturing (WAAM)-fabricated Inconel 625 alloy has been examined. The research was done on the microstructure, mechanical characteristics, and impact of the solidification rate on the characteristics of the manufactured specimens for the Inconel 625 alloy. Microstructural analysis has shown that the specimen’s layers have varying microstructures. The bottom layer exhibits a blocky or equiaxed microstructure because of the faster solidification rate, while the upper zone generated elongated and discontinuous dendrites because of the slower solidification rate. This difference in the microstructure in the top and bottom zones directly influence the ultimate tensile strength, where the bottom zone has more tensile and yield strength than the top zone. Also, the presence of cracks in the top zone, which is found during the fractography test, also correlated the top zone’s ultimate tensile strength.
Go to article

Authors and Affiliations

K. Saravanakumar
1
ORCID: ORCID
V.G. Balaji
1
T. Srijha
1
V. Sanjay
1
K. Thatchuneswaran
1

  1. PSG College of Technology, Department of Production Engineering, Coimbatore-641004, India