Details

Title

Inoculation of Gray Cast Iron Intended for Large Scale and Heavy Weight Castings of Bottom Plates and Counterweights Manufactured in the Krakodlew S.A.

Journal title

Archives of Foundry Engineering

Yearbook

2022

Volume

vol. 22

Issue

No 3

Authors

Affiliation

Szczęsny, A. : AGH University of Science and Technology, Department of Foundry, ul. Reymonta 23, 30-059 Kraków, Polska ; Kopyciński, D. : AGH University of Science and Technology, Department of Foundry, ul. Reymonta 23, 30-059 Kraków, Polska ; Guzik, E. : AGH University of Science and Technology, Department of Foundry, ul. Reymonta 23, 30-059 Kraków, Polska

Keywords

Heavy castings ; Large scale casting ; Grey cast iron ; Inoculation

Divisions of PAS

Nauki Techniczne

Coverage

19-24

Publisher

The Katowice Branch of the Polish Academy of Sciences

Bibliography

[1] Benedetti, M., Torresani, E., Fontanari, V. & Lusuardi, D. (2017). Fatigue and fracture resistance of heavy-section ferritic ductile cast iron. Metals. 7(3), 88.
[2] Dorula, J., Kopyciński, D., Guzik, E., Szczęsny, A. & Gurgul, D. (2021). The influence of undercooling ΔT on the structure and tensile strength of grey cast iron. Materials. 14(21), 6682.
[3] Wang, Q., Cheng, G. & Hou, Y. (2020). Effect of titanium addition on as-cast structure and high-temperature tensile property of 20Cr-8Ni stainless steel for heavy castings. Metals. 10(4), 529.
[4] Wang, Q., Chen, S. & Rong, L. (2020). -Ferrite formation and its effect on the mechanical properties of heavy-section AISI 316 stainless steel casting. Metallurgical and Materials Transactions A. 51, 2998-3008.
[5] Kalandyk, B., Zapała, R., Sobula, S., Górny, M. & Boroń, Ł. (2014) Characteristics of low nickel ferritic-austenitic corrosion resistant cast steel. Metalurgija-Metallurgy. 53(4), 613-616.
[6] Kalandyk, B. & Zapała, R. (2013). Effect of high-manganese cast steel strain hardening on the abrasion wear resistance in a mixture of SiC and water. Archives of Foundry Engineering. 13(4), 63-66.
[7] Tęcza, G. & Zapała, R. (2018). Changes in impact strength and abrasive wear resistance of cast high manganese steel due to the formation of primary titanium carbides. Archives of Foundry Engineering. 18(1), 119-122.
[8] Tęcza, G. & Garbacz-Klempka, A. (2016). Microstructure of cast high-manganese steel containing titanium. Archives of Foundry Engineering. 16(4), 163-168.
[9] Celis, M., Domengès, B., Hug, E. & Lacaze, J. (2018). Analysis of nuclei in a heavy-section nodular iron casting. Materials Science Forum. 925, 173-180.
[10] Kopyciński, D., Siekaniec, D., Szczęsny, A., Sokolnicki, M. & Nowak, A. (2016). The Althoff-Radtke test adapter for high chromium cast iron. Archives of Foundry Engineering. 16(4), 74-77.
[11] Szczęsny, A., Kopyciński, D., Guzik, E. Soból, G., Piotrowski, K., Bednarczyk, P. & Paul, W. (2020). Shaping of ductile cast iron dedicated for slag ladle. Acta Metallurgica Slovaca. 26, 74-77. https://doi.org/10.36547/ams.26.2.312
[12] Mourad, M.M. & El-Hadad, S. (2015). Effect of processing parameters on the mechanical properties of heavy section ductile iron. Journal of Metallurgy. 2015, 1-11.
[13] Foglio, E., Gelfi, M., Pola, A. & Lusuardi, D. (2017). Effect of shrinkage porosity and degenerated graphite on fatigue crack initiation in ductile cast iron. Key Engineering Materials. 754, 95-98.
[14] Kavicka, F., Sekanina, B., Stetina, J., Stransky, K., Gontarev, V. & Dobrovska, J. (2009). Numerical optimization of the method of cooling of a massive casting of ductile cast-iron. Materials and Technology. 43, 73-78.

Date